- ad air dried 空干基
- ar as received 收到基
- daf dry ash free 干燥无灰基
- csn crucible swell number 坩埚膨胀序数
- cv calorific value 热值
- ddpm dial divisions per minute 旋转速度用刻度盘
- fc fixed carbon 固定碳
- hgi hardgrove grindability index 哈氏可磨指数
- im inherent moisture 内在水分
- kcal/kg kilocalories per kilogram 千卡/千克
- m40 percentage of sample remaining over 40mm after a rotating drum test 抗碎强度指标
- m10 percentage of sample under 10mm in size after a rotating drum test 耐磨强度
- max maximum 最大值
- mm millimeters 毫米
- p phosphorus 磷
- pci (coal for) pulverized coal injection 喷吹煤
- tm total moisture 全水
- ts total sulphur 全硫
- vm volatile matter 挥发份